Vapour smoothing is a controlled finishing process that reduces surface roughness and seals micro-porosity on SLS Nylon 12 parts. It treats external surfaces and internal channels evenly, keeps functional geometry, and gives a finish closer to injection-molded parts. Agile Manufacturing offers vapour smoothing on SLS Nylon 12 for functional prototypes and end-use parts across Canada.
If you’re using SLS Nylon 12 for functional prototypes or end-use components, vapour smoothing can transform your parts into production-ready results with a premium finish, without changing your geometry or adding labour-intensive manual finishing steps.
What Is Vapour Smoothing for SLS Nylon 12?
Vapour smoothing is a controlled finishing process that reduces surface roughness and seals micro-porosity on SLS Nylon 12 parts. The result is a smoother, more consistent surface, often closer to injection-molded aesthetics, while keeping the benefits of SLS: complex geometries, durable nylon performance and efficient batch production.
Raw SLS vs Vapour Smoothed SLS Nylon 12
| Property | Raw SLS Nylon 12 | Vapour smoothed SLS Nylon 12 |
| Surface feel | Slightly grainy, powder texture | Smooth, sealed, closer to injection-molded |
| Porosity | Micro-porous surface | Sealed surface |
| Sealing | Not watertight or airtight by default | Improved watertight and airtight sealing |
| Cleaning | Can trap residue | Easier to clean |
| Internal channels | Not finished | Finished evenly with external surfaces |
| Dyeing and painting | Uneven uptake possible | More even, richer color |
| Geometry | As printed | Functional geometry maintained |
Why Vapour Smoothing Is a Game-Changer for SLS Parts
Enhanced Part Properties
- Superior surface finish: A cleaner, more uniform surface that looks and feels “finished,” not “printed.”
- Improved mechanical performance in real-world handling: A sealed surface can reduce weak points created by surface porosity and improve durability in many applications.
- Watertight and airtight sealing: Great for housings, manifolds, covers, ducts and parts that need improved containment.
- Reduced bacterial adhesion and easier cleaning: Smoother, less porous surfaces are often easier to clean and may help reduce areas where residue can build up, which is useful for products that need hygienic handling.
- UV resistance: When paired with appropriate secondary finishing, such as coatings or dyes, vapour-smoothed parts can be better prepared for outdoor or UV-exposed use.
Manufacturing and Design Advantages
- Non-line-of-sight finishing for complex geometries: Unlike sanding, painting or manual finishing, vapour smoothing can uniformly treat both external surfaces and internal channels, even in complex lattices and intricate passages. This is ideal for SLS designs that are hard to reach.
- Maintained dimensional accuracy: The process is designed to preserve functional geometry and fit where tight tolerances matter.
- Better results with dyeing and painting: A smoother, sealed surface typically accepts dyeing and painting more evenly, producing richer, more uniform color and a more consistent final look.
Where Vapour-Smoothed SLS Nylon 12 Shines
Vapour-smoothed Nylon 12 is commonly used for parts that need a more refined finish without sacrificing strength and design freedom:
| Industry | Typical parts |
| Automotive | Ducts, housings, brackets, interior components, low-volume production |
| Medical devices and accessories | Functional housings, handles, covers (application dependent) |
| Consumer goods | Premium prototypes, product shells, enclosures, wearable components |
| Industrial | Jigs, fixtures, tooling aids, covers, airflow components |
If your application has regulatory requirements or special performance needs, include them in your RFQ so we can recommend the right finishing approach. Comparing processes? Read SLA vs SLS: Which is Best for You?
How to Request a Vapour Smoothing Quote
Request a quote from Agile Manufacturing and include:
- Part quantity and target lead time
- Intended use (prototype or end-use)
- Any sealing needs (watertight or airtight)
- Any post-finishing needs (dyeing or painting)
- Drawings or 3D files (STEP preferred)
- Critical fits or tolerances to protect during finishing
Current Offers
Agile runs vapour smoothing promotions from time to time, such as complimentary vapour smoothing on SLS Nylon 12 orders in January 2026. Mention vapour smoothing when you request an SLS Nylon 12 quote to check for current offers.
Frequently Asked Questions
Vapour smoothing is a controlled finishing process that reduces surface roughness and seals micro-porosity on SLS Nylon 12 parts, giving a smoother, more consistent finish closer to injection-molded parts.
Yes. Vapour smoothing is a non-line-of-sight finishing method, so it treats internal and external surfaces more uniformly than many manual finishing methods.
The process is intended to maintain dimensional accuracy. If you have critical fits or tolerances, call them out in your quote request so finishing can be evaluated appropriately.
Vapour smoothing seals micro-porosity, which improves watertight and airtight sealing for housings, manifolds, covers and ducts. State your sealing needs in your quote request.
Yes. A sealed, smoother surface often produces more even dye uptake and better paint consistency, leading to a more uniform appearance.
Automotive ducts and housings, medical device housings and handles, consumer product shells and wearables, and industrial jigs, fixtures and airflow components.
Yes. Agile Manufacturing offers vapour smoothing on SLS Nylon 12 parts. Mention it when you request an SLS quote to check for current offers.